Introduction to Heat Resistant Alloys

Share:

More Articles

Trade Shows

Come talk to a Rolled Alloys representative in person about your project. You can find us at these trade shows.

Read More »

History and Uses of Alloy 800

Discover the evolution of Alloy 800, from its origins during the 1950s to modern derivatives like Alloy 800H/800HT. Learn about its high-temperature strength, petrochemical applications, and commercial availability today.

Read More »

Quote, Buy, Track!

We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!

We have been supporting the heat-resistant alloy market for over 70 years. Many different industries, such as thermal processing, chemical processing, and power generation, depend on the capabilities of these alloys to perform day-to-day activities.

In this webinar, we will explore the world of wrought heat-resistant alloys. The listener will be introduced to commonly utilized heat-resistant alloys, factors to consider when selecting a heat-resistant alloy, and some industrial applications within specific industries. 

Presentation Slides

An Introduction to Heat Treat Alloys

Exploring the World of High-Temperature Alloys 

Welcome to Rolled Alloys’ Webinar Series 

Hello and welcome to Rolled Alloys’ second webinar in our ongoing series. In today’s session, we’re delving into the fascinating world of heat-resistant alloys. Whether you’re a materials enthusiast or someone seeking specific solutions for high-temperature applications, we’ve got you covered. 

In this blog post, we will cover key takeaways from the webinar, explore the fundamental aspects of heat-resistant alloys, and discuss their applications. We will also touch upon some important considerations when choosing the right materials for your specific needs. 

Rolled Alloys: Your Trusted Global Supplier 

Before we dive into the world of heat-resistant alloys, it’s essential to know who we are. Rolled Alloys is a global supplier specializing in high-performance alloys. Our offering includes state-of-the-art material processing, an exceptional e-commerce platform, and a team of metallurgical experts to assist you. We provide a wide range of alloys, including nickel alloys, stainless steels, duplex, titanium, cobalt, and various forms such as plates, sheets, and bars. 

Meet the Expert: Hugh Thompson

Our speaker for today is Hugh, an Application Engineer with Rolled Alloys. With a Bachelor of Science in Mechanical Engineering from the University of Toledo School of Engineering, Hugh has been a valuable member of our team since 2019. His responsibilities include conducting failure analyses, addressing technical inquiries, and assisting customers in material selection for specific applications and processes. He’s also actively involved with organizations like ASME, MTI, and the Association for Materials Protection and Performance. 

What Are Heat-Resistant Alloys? 

Heat-resistant alloys are a special group of materials designed for high-temperature environments. These alloys contain a minimum of 12% chromium to form a protective chromium oxide layer at high temperatures. Additional elements such as carbon, nitrogen, nickel, silicon, and aluminum enhance their properties. Rare earth metals are also incorporated to improve oxide adherence. 

Some common heat-resistant alloys include,

Factors to Consider When Selecting Heat-Resistant Alloys 

  1. Oxidation Resistance: Heat-resistant alloys with at least 12% chromium can form an oxide layer that protects them at high temperatures. Beyond the oxidation threshold, they become porous and brittle.
  2. Creep Strength: Creep is time-dependent deformation at elevated temperatures and constant stress. High creep strength alloys retain their shape, making them ideal for high-temperature applications.
  3. Carburizing and Nitriding: These processes introduce carbon and nitrogen into the material’s surface, enhancing wear resistance. Alloys with high nickel content are better suited for these environments.
  4. Vacuum Processing: The process environment should be void of oxygen. Therefore, high temperature oxidation does not tend to be a concern. 

  

Common Applications of Heat-Resistant Alloys

  • Thermal Processing: Used for bar baskets, serpentine grids, radiant tubes, and retorts.
  • Chemical Processing: Used for flair tips, piping, steam methane reformers, and heat exchangers.
  • Galvanizing Lines: Used for their corrosion resistance.
 

Heat-resistant alloys are also used in a wide range of industries including:

  • Power Generation
  • Aerospace
  • Oil and Gas
  • Steel Manufacturing

  

Conclusion 

Heat-resistant alloys are at the heart of numerous high-temperature applications. Understanding their properties and how they behave in various environments is crucial to making the right material selection. 

We hope this blog post has provided you with valuable insights into the world of heat-resistant alloys. If you have any questions or need further assistance, please don’t hesitate to reach out to us. You can contact us via email or phone, and we’ll be happy to help. 1-800-521-0332 or email us metallurgical-help@rolledalloys.com

Buy Online Anytime

Our dashboard makes it even easier to shop online anytime from anywhere. Quote, buy, and track 24 hours a day at rolledalloys.com.

Events

Trade Shows

Come talk to a Rolled Alloys representative in person about your project. You can find us at these trade shows.

March Mania
General

March Mania 2025

Every Online Order in March is a Chance to Win One of 8 Great Prizes!

Technical Article

History and Uses of Alloy 800

Discover the evolution of Alloy 800, from its origins during the 1950s to modern derivatives like Alloy 800H/800HT. Learn about its high-temperature strength, petrochemical applications, and commercial availability today.

Privacy Overview

This website uses cookies so that we can provide you with the best user experience possible. Cookie information is stored in your browser and performs functions such as recognising you when you return to our website and helping our team to understand which sections of the website you find most interesting and useful.