NICKEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
![](https://www.rolledalloys.com/wp-content/uploads/precipitates-wrought-duplex-stainless-steels-rolled-alloys.jpg)
Quality of Microstructure of Duplex Stainless Steels
Duplex stainless steels typically have 50% of both austenite and ferrite in their microstructure. It is necessary to have good
![](https://www.rolledalloys.com/wp-content/uploads/flat-bar-rolled-alloys-1.jpg)
Flat Bar or Gauered Flat Bar from Plate
Discover the difference between flat bars and gauered flat bars cut from plates. Learn about their dimensional tolerances and the
![](https://www.rolledalloys.com/wp-content/uploads/ra330-metal-dusting-corrosion-Rolled-Alloys.jpg)
Metal Dusting
Metal Dusting is a hazard when using heat-treat carburizing furnaces and petrochemical equipment. Explore how high-chromium alloys thwart this destructive
![](https://www.rolledalloys.com/wp-content/uploads/stainless-steel-process-rolled-alloys.jpg)
Manganese Substitution Grades of Stainless Steel
Explore the evolution of stainless steel with manganese substitution grades, offering cost-effective solutions for industries like appliances and food equipment.
625
Inconel® 625 is a nickel-base alloy used both for its high strength and outstanding aqueous corrosion resistance. The strength of alloy 625 is primarily a solid solution effect from molybdenum and niobium.
Share This Page
- High creep-rupture strength
- Oxidation resistant to 1800°F
- Good fatigue resistance
- Excellent weldability
- Outstanding resistance to chloride pitting and crevice corrosion
- Immune to chloride ion stress corrosion cracking
- Resistant to seawater under both flowing and stagnant conditions and under fouling
UNS: N06625
W. NR.: 2.4856
ASTM: B 443 GR 1, B 446 GR 1
ASME: SB 443 GR 1, SB 446 GR 1
AMS: 5599, 5666, 5837
NACE: MR0175
ISO: 15156
- Inconel® 625
- Alloy 625
- Nickel 625
- 625 Plate
- 625 Round Bar
- 625 Sheet
- Aircraft ducting systems
- Jet engine exhaust systems
- Engine thrust-reverser systems
- Bellows and expansion joints
- Turbine shroud rings
- Flare stacks
- Seawater components
- Chemical process equipment handling mixed acids both oxidizing and reducing.