DUPLEX STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
![](https://www.rolledalloys.com/wp-content/uploads/precipitates-wrought-duplex-stainless-steels-rolled-alloys.jpg)
Quality of Microstructure of Duplex Stainless Steels
Duplex stainless steels typically have 50% of both austenite and ferrite in their microstructure. It is necessary to have good
![](https://www.rolledalloys.com/wp-content/uploads/flat-bar-rolled-alloys-1.jpg)
Flat Bar or Gauered Flat Bar from Plate
Discover the difference between flat bars and gauered flat bars cut from plates. Learn about their dimensional tolerances and the
![](https://www.rolledalloys.com/wp-content/uploads/ra330-metal-dusting-corrosion-Rolled-Alloys.jpg)
Metal Dusting
Metal Dusting is a hazard when using heat-treat carburizing furnaces and petrochemical equipment. Explore how high-chromium alloys thwart this destructive
![](https://www.rolledalloys.com/wp-content/uploads/stainless-steel-process-rolled-alloys.jpg)
Manganese Substitution Grades of Stainless Steel
Explore the evolution of stainless steel with manganese substitution grades, offering cost-effective solutions for industries like appliances and food equipment.
2507
2507 (UNS S32750) is a super duplex stainless steel designed for applications which require exceptional strength and corrosion resistance. 2507 is a 25% chromium, 4% molybdenum, and 7% nickel alloy resulting in excellent resistance to chloride pitting and crevice corrosion attack. The duplex structure provides 2507 with exceptional resistance to pitting and chloride stress corrosion cracking.
Usage of 2507 should be limited to applications below 600° F (316° C). Extended exposure to elevated temperatures can reduce its toughness and corrosion resistance.
- High resistance to chloride stress corrosion cracking
- Strong resistance to chloride pitting and crevice corrosion
- High strength
- Strong general corrosion resistance
- Suggested for applications up to 600° F
- Good weldability / workability
- Resistant to pitting and crevice corrosion in seawater
UNS: S32750
W. NR.: 1.4410
ASTM: A 240, A 276, A 479, A 182
ASME: SA 240, SA 276, SA 479, SA 182
NACE: MRO175
ISO: 15156
- Desalination Equipment
- Chemical process pressure vessels, piping and heat exchangers
- Marine Applications
- Flue Gas Scrubbing Equipment
- Pulp & Paper Mill Equipment
- Offshore Oil production/technology
- Oil and gas industry equipment