STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
![](https://www.rolledalloys.com/wp-content/uploads/precipitates-wrought-duplex-stainless-steels-rolled-alloys.jpg)
Quality of Microstructure of Duplex Stainless Steels
Duplex stainless steels typically have 50% of both austenite and ferrite in their microstructure. It is necessary to have good
![](https://www.rolledalloys.com/wp-content/uploads/flat-bar-rolled-alloys-1.jpg)
Flat Bar or Gauered Flat Bar from Plate
Discover the difference between flat bars and gauered flat bars cut from plates. Learn about their dimensional tolerances and the
![](https://www.rolledalloys.com/wp-content/uploads/ra330-metal-dusting-corrosion-Rolled-Alloys.jpg)
Metal Dusting
Metal Dusting is a hazard when using heat-treat carburizing furnaces and petrochemical equipment. Explore how high-chromium alloys thwart this destructive
![](https://www.rolledalloys.com/wp-content/uploads/stainless-steel-process-rolled-alloys.jpg)
Manganese Substitution Grades of Stainless Steel
Explore the evolution of stainless steel with manganese substitution grades, offering cost-effective solutions for industries like appliances and food equipment.
RA 253 MA®
The High Strength Heat Resistant Stainless Steel
RA 253 MA® was developed when the need for a heat resistant stainless steel with high strength, while maintaining good oxidation resistance was present in the industry. The lean 11% nickel content of RA 253 MA is a key contributor to being cost effective and stable. With the addition of rare earth elements, RA 253 MA still performs well at temperatures up to 2000°F (1093°C), similar to that of 310 stainless steel.
Performance Profile
RA 253 MA is a lean austenitic heat resistant alloy with high strength and outstanding oxidation resistance. It offers an excellent combination of creep strength along with excellent resistance to oxidation, sulfidation, and erosion at high temperatures in an alloy containing just 11% nickel. Because of its lean chemistry, RA 253 MA is very economical compared to most heat resistant alloys.
RA 253 MA obtains its heat resistant properties by tight control of micro alloy additions. The use of cerium in combination with silicon results in superior oxidation resistance to 2000°F (1093°C). Nitrogen, carbon, and cerium combine to provide creep rupture strength that is double that of type 310 and 309 stainless at 1600°F (871°C).
- Oxidation resistance to 2000°F (1093°C)
- Good resistance to sulfidation
- Superior strength at elevated temperatures
- Good resistance to high temperature abrasion
UNS: S30815
W. NR.: 1.4835
ASTM: A 240, A 276, A 312, A 479
ASME: SA 182, SA 312
- Boiler Nozzels
- Corrugated Boxes
- Cyclones
- Bar Baskets
- Radiant Tubes