Quality of Microstructure of Duplex Stainless Steels
Duplex stainless steels typically have 50% of both austenite and ferrite in their microstructure. It is necessary to have good
![](https://www.rolledalloys.com/wp-content/uploads/flat-bar-rolled-alloys-1.jpg)
Flat Bar or Gauered Flat Bar from Plate
Discover the difference between flat bars and gauered flat bars cut from plates. Learn about their dimensional tolerances and the
![](https://www.rolledalloys.com/wp-content/uploads/ra330-metal-dusting-corrosion-Rolled-Alloys.jpg)
Metal Dusting
Metal Dusting is a hazard when using heat-treat carburizing furnaces and petrochemical equipment. Explore how high-chromium alloys thwart this destructive
![](https://www.rolledalloys.com/wp-content/uploads/stainless-steel-process-rolled-alloys.jpg)
Manganese Substitution Grades of Stainless Steel
Explore the evolution of stainless steel with manganese substitution grades, offering cost-effective solutions for industries like appliances and food equipment.
N-60
N-60 stainless is known for its excellent galling resistance, even at elevated temperatures. The additions of 4% silicon and 8% manganese inhibit wear, galling, and fretting. It is commonly used for various fasteners and pins that require strength and resistance to galling. It maintains decent strength up to temperatures of 1800°F and has oxidation resistance similar to that of 309 stainless steel. The general corrosion resistance is between that of 304 and 316 stainless steel.
- Wear and galling resistant alloy
UNS: S21800
ASTM: A 193, A 193 CLASS 1C, A 276, A 479
ASME: SA 193, SA 479
AMS: 5848
Nitronic 60
- Fasteners
- Pins and bushings
- Wear rails
- Roller bearings
- Pump components