![](https://www.rolledalloys.com/wp-content/uploads/precipitates-wrought-duplex-stainless-steels-rolled-alloys-300x238.jpg)
Quality of Microstructure of Duplex Stainless Steels
Duplex stainless steels typically have 50% of both austenite and ferrite in their microstructure. It is necessary to have good control of…
![](https://www.rolledalloys.com/wp-content/uploads/flat-bar-rolled-alloys-1-300x200.jpg)
Flat Bar or Gauered Flat Bar from Plate
Discover the difference between flat bars and gauered flat bars cut from plates. Learn about their dimensional tolerances and the importance of edge and corner conditions in stainless and nickel alloy products.
![](https://www.rolledalloys.com/wp-content/uploads/ra330-metal-dusting-corrosion-Rolled-Alloys-300x288.jpg)
Metal Dusting
Metal Dusting is a hazard when using heat-treat carburizing furnaces and petrochemical equipment. Explore how high-chromium alloys thwart this destructive process, safeguarding crucial industrial assets against disintegration at temperatures ranging from 800 to 1700°F.
![](https://www.rolledalloys.com/wp-content/uploads/stainless-steel-process-rolled-alloys-300x200.jpg)
Manganese Substitution Grades of Stainless Steel
Explore the evolution of stainless steel with manganese substitution grades, offering cost-effective solutions for industries like appliances and food equipment.
![](https://www.rolledalloys.com/wp-content/uploads/Plate-Thickness-Varations-Rolled-Alloys-300x200.jpg)
Plate Thickness Variations
Plate Thickness Variation Back To All Articles Share: More Articles Quote, Buy, Track! We make it easy to get instant pricing and purchase your metal
![](https://www.rolledalloys.com/wp-content/uploads/Duplex-Stainless-Steel-Webinar-Graphic-300x169.png)
Best Practices When Using Duplex Stainless Steels
Best Practices When Using Duplex Stainless Steel Back To All Articles Share: More Articles Quote, Buy, Track! We make it easy to get instant pricing