STAINLESS STEEL
Quote, Buy, Track!
We make it easy to get instant pricing and purchase your metal at the click of a button. Track your order progress, get notified when it ships, and follow your shipment online until it’s delivered. It’s that easy!
Latest Articles
![](https://www.rolledalloys.com/wp-content/uploads/precipitates-wrought-duplex-stainless-steels-rolled-alloys.jpg)
Quality of Microstructure of Duplex Stainless Steels
Duplex stainless steels typically have 50% of both austenite and ferrite in their microstructure. It is necessary to have good
![](https://www.rolledalloys.com/wp-content/uploads/flat-bar-rolled-alloys-1.jpg)
Flat Bar or Gauered Flat Bar from Plate
Discover the difference between flat bars and gauered flat bars cut from plates. Learn about their dimensional tolerances and the
![](https://www.rolledalloys.com/wp-content/uploads/ra330-metal-dusting-corrosion-Rolled-Alloys.jpg)
Metal Dusting
Metal Dusting is a hazard when using heat-treat carburizing furnaces and petrochemical equipment. Explore how high-chromium alloys thwart this destructive
![](https://www.rolledalloys.com/wp-content/uploads/stainless-steel-process-rolled-alloys.jpg)
Manganese Substitution Grades of Stainless Steel
Explore the evolution of stainless steel with manganese substitution grades, offering cost-effective solutions for industries like appliances and food equipment.
310
Excellent resistance to oxidation under mildly cyclic conditions through 2000°F characterizes 310 stainless. Because of its high chromium and medium nickel contents, 310 has good resistance to sulfidation and other forms of hot corrosion. 310 is widely used in moderately carburizing atmospheres such as encountered in petrochemical environments. The more severely carburizing atmospheres of industrial heat treating furnaces require RA330® or RA333®. 310 is not suggested for the severe thermal shock of repeated liquid quenching.
Often in many product forms, the grain size and carbon content can meet both the 310S and 310H requirements. 310 is often used at cryogenic temperatures, with excellent toughness to -450°F, and low magnetic permeability. 310 has a machinability rating of 42% relative to AISI B1112 steel. When using high speed steel tooling, this equates to about 70 surface feet per minute. Forming operations should be performed at room temperature whenever possible. Welding with AWS E310-15 electrodes or ER310 bare wire is suggested.
- Oxidation resistance to 2000°F
- Moderate strength at high temperature
- Resistance to hot corrosion
- Strength and toughness at cryogenic temperatures
UNS: S31008, S31009
W. NR.: 1.4845
EN: 10095
ASTM: A 240, A 276, A 312, A 479
ASME: SA 240, SA 276, SA 312, SA 479
AMS: 5521, 5651
- Flare tips
- Fluidized bed coal combustors
- Radiant tubes
- Tube hangers for petroleum refining and steam boilers
- Coal gasifier internal components
- Thermowells
- Refractory anchor bolts
- Burners, combustion chambers
- Retorts, muffles, annealing covers
- Food processing equipment
- Cryogenic structures